Research Article

Preparation of Amino-Modified PAN Fibers with Triethylenetetramine as Aminating Reagents and Their Application in Adsorption

Table 1

Surface of AMPAN fiber prepared at different temperatures.

FiberFiber 150°CFiber 160°CFiber 170°CFiber 180°C

Surface area (m2/g)0.8780.9761.0481.238