Enhanced Photocatalytic Activity of W-Doped and W-La-Codoped TiO2 Nanomaterials under Simulated Sunlight

Figure 7

(a) Decolorization profiles of MO in the presence of (A) pure TiO2, (B) 0.8% W/TiO2, and (C) 4% La/W/TiO2 in the dark. Photocatalytic decolorization curves of MO over the catalysts under simulated sunlight irradiation: (A) blank, (B) P25, (C) pure TiO2, (D) 0.4% W/TiO2, (E) 0.6% W/TiO2, (F) 0.8% W/TiO2, (G) 1.0% W/TiO2, and (H) 1.2% W/TiO2 in (b) and (A) 0.8% W/TiO2, (B) 1% La/W/TiO2, (C) 2% La/W/TiO2, (D) 3% La/W/TiO2, (E) 4% La/W/TiO2, and (F) 5% La/W/TiO2 in (c). (d) PL spectra of the (A) pure TiO2, (B) 0.8% W/TiO2, and (C) 4% La/W/TiO2 nanomaterials.
(a)
(b)
(c)
(d)