Research Article
Wettability Investigation of UV/O3 and Acid Functionalized MWCNT and MWCNT/PMMA Nanocomposites by Contact Angle Measurement
Table 4
Surface energy calculation of treated MWCNT/PMMA nanocomposites using GvOC model.
| Sample | (mJ/m2) | (mJ/m2) | (mJ/m2) | (mJ/m2) | (mJ/m2) |
| Raw CNT | 11.33 | 10.15 | 1.18 | 1.86 | 0.19 | UV/O3 30 min | 22.72 | 20.79 | 1.93 | 0.45 | 2.07 | UV/O3 60 min | 136.26 | 116.00 | 120.26 | 11.31 | 77.77 | UV/O3 120 min | 146.93 | 2.75 | 4.17 | 0.99 | 4.39 | Acid 6 hours | 12.45 | 5.30 | 7.15 | 1.66 | 7.69 | Acid 12 hours | 18.80 | 7.66 | 11.14 | 2.68 | 11.58 | Acid 24 hours | 24.82 | 11.54 | 13.28 | 3.50 | 12.59 |
|
|