Grafting Carbon Nanotubes on Glass Fiber by Dip Coating Technique to Enhance Tensile and Interfacial Shear Strength

Figure 3

CNT coated GF soaked in 1 mg/mL CNT suspension with soaking time of (a) 60 min and (b) 180 min.