Research Article
Fabrication of Coatings on the Surface of Magnesium Alloy by Plasma Electrolytic Oxidation Using ZrO2 and SiO2 Nanoparticles
Figure 12
Scratch testing data for the sample with PEO coating containing ZrO2 nanoparticles and image of the scratch after the experiment: lines correspond to the values of loads, at which scaling of coatings parts (а) and its plastic abrasion down to metal () (b) occur. 1: applied load, 2: depth of indenter penetration at load, 3: acoustic emission, 4: friction force, and 5: residual depth of indenter penetration after unloading.