Research Article
Photocatalytic Oxidation of Trichloroethylene in Water Using a Porous Ball of Nano-ZnO and Nanoclay Composite
Figure 7
Effect of initial concentration of TCE on photocatalytic degradation (initial concentration of TCE = 1–20 mg⋅L−1; nano-ZnO-laponite loading = 30 g; pH = 7.0; irradiation time = 60 min; and UVC intensity = 8.4 mW⋅cm−2).