Weight loss of linoleic and stearic acids with 75V2O5-15B2O3-10P2O5 glass heat-treated at 275°C.

Heating processLinoleic acidStearic acid
Start temp. of weight lossFinish temp. of weight lossStart temp. of weight lossFinish temp. of weight loss

Annealed254.19356.05235.56378.67
275°C/1 h245.24324.15233.23341.75
275°C/3 h244.02330.92233.55350.02
275°C/5 h244.23340.96233.62362.16