Research Article

Oxidation and Corrosion Behavior of Nanolaminated MAX-Phase Ti2AlC Film Synthesized by High-Power Impulse Magnetron Sputtering and Annealing

Table 3

Corrosion analyses from potential dynamic polarization curves in the 3.5 wt.% NaCl aqueous solution.

SUS304
substrate
Amorphous matrix
Ti-Al-C
MAX-phase
Ti2AlC

(A/cm2)1.91 × 10−51.44 × 10−65.82 × 10−8
(V vs. SCE)−0.529−0.618−0.301