Fabrication and Characterization of Cellulose Acetate/Montmorillonite Composite Nanofibers by Electrospinning

Table 1

The residue and decomposition temperature at onset and 20% rate of pure MMT and nanofibers (pure CA, CA/MMT-1, CA/MMT-3, CA/MMT-5, CA/MMT-7, and CA/MMT-9).

Materials onset (°C) 20% (°C)Residue at 500°C (%)

Pure CA28034013
Pure MMT28038065
CA/MMT-127533013
CA/MMT-327532514
CA/MMT-527031515
CA/MMT-727031017
CA/MMT-927031018