Figure 12

Typical example of the EDX analysis on a fractured grain using spot measurements starting from the center of the grain (Point 0) as a function of distance from the center. Sample characteristics: [Ni] = 0.13 M, [P] = 1.26 M, heat treatment temperature °C, heating rate °C/min, and annealing time min followed by cooling in air. Scale bar = 2 μm.