The composition of the bath for electroless Ni plating.

Bath compositionConcentration

NiSO4·6H2O0.10 M
NaH2PO3·H2O0.23 M
Na3C6H5O7·2H2O0.07 M
NaC2H3O20.06 M
Pb(CH3COO)2·2H2O0.004 mM

Deposition conditionValue

Temperature75°C
pH10