Research Article
Effect of Pore Thickness and the State of Polarization on the Optical Properties of Hexagonal Nanoarray of Au/Nanoporous Anodic Alumina Membrane
Figure 2
FE-SEM and AFM images of NAAMs anodized for ((a), (b)) 5 min and ((c), (d)) 10 min sputtered with Au for 40 sec under the same conditions.
(a) |
(b) |
(c) |
(d) |