Research Article

Luminescence Performance of Yellow Phosphor SrxBa1−xTiO3: Eu3+, Gd3+ for Blue Chip

Figure 3

SEM images of SrTiO3: Eu3+, Gd3+ calcined at 1100°C for 3 h.