Research Article

Influence of Milling Conditions on the Hydriding Properties of Mg-C Nanocomposites

Figure 3

High-pressure DSC plots (25 bars, 5 K/min) for the Mg-CB composites ((a) milled 15 h with heptane, (b) 35 h milled with heptane, (c) 35 h milled at dry conditions, (d) 15 h high energy milled, and (e) milled from MgH2).