Research Article
Superhydrophobic Polyimide via Ultraviolet Photooxidation: The Evolution of Surface Morphology and Hydrophobicity under Different Ultraviolet Intensities
Figure 5
SEM image and corresponding EDS mappings of O (b) and C (c) of UV-treated PI (10 mW/cm2, 72 h). The images were taken at the same position of the sample at the same scale.
(a) |
(b) |
(c) |