Research Article

WO3 Nanoplates Film: Formation and Photocatalytic Oxidation Studies

Figure 5

Photocatalytic degradation of MO aqueous dye solution under solar irradiation over anodic WO3 samples synthesized in an ethylene glycol containing different NH4F at 60 V for 1 h: (a) 0.7 wt%, (b) 0.5 wt%, (c) 0.3 wt%, (d) 0.1 wt%, and (e) control sample (blank sample).