(a)
(b)
(c)
(d)
Figure 5: TEM images of as-prepared Co3O4 (a), Pr6O11/Co3O4 (b), Sm2O3/Co3O4 (c), and Tb4O7/Co3O4 (d) being prepared by the coprecipitation method and calcined at 500°C.