Research Article

Magnetism of FePt Nanoclusters in Polyimide

Figure 1

(a) SEM photographs of KHN-FePt. WAXS of KHN-FePt. (b) Not annealed KHN-FePt (thick black line) and KHN-FePt annealed at 400°C for 10 minutes by RTA (thin gray line). (c)WAXS of as-deposited KHN-FePt (thick black line), of KHN-FePt annealed at 460°C for 1 h in (parallel) = 10 kOe (thin black line), and of KHN-FePt annealed at 460°C, for 1 h, in (perpendicular) = 10 kOe (thick gray line).
(a)
(b)
(c)