Degradation of FBL Dye Wastewater by Magnetic Photocatalysts from Scraps

Figure 5

XRD pattern of Mn-Zn ferrite powder (a), Mn-Zn ferrite sintered at 1200°C (N2) (b), and Mn-Zn ferrite/TiO2 (N2, 500°C) (c).
(a)
(b)
(c)