Effects of Preparation Conditions on the CuInS2 Films Prepared by One-Step Electrodeposition Method

Figure 3

XRD (a) and Raman spectra (b) of CuInS2 films obtained at S contents 0.5, 1, 1.25, and 1.5 g.