Importance of the Electrolyte in Obtaining Porous Silicon and How It Modifies the Optical and Structural Proprieties: Optical and Microstructural Investigation

Table 1

Conditions for the PS preparation.

Sample Anodization time (min)Electrolyte

M1101 : 2 (HF/CH3-CH2-OH)
M2151 : 2 (HF/CH3-CH2-OH)
M3102 : 1 : 1 (H2O2/HF/CH3-CH2-OH)
M4152 : 1 : 1 (H2O2/HF/CH3-CH2-OH)