Research Article

Crystallization Behavior of Phosphate Glasses with Hydrophobic Coating Materials

Figure 7

SEM images of PFTL glasses heated under different conditions: (a) PFTL0, (b) PFTL1, (c) PFTL2, and (d) PFTL3 glasses heated at 800°C for 5 min and (e) PFTL0, (f) PFTL1, (g) PFTL2, and (h) PFTL3 glasses heated at 850°C for 5 min.
(a)
(b)
(c)
(d)
(e)
(f)
(g)
(h)