Research Article
Influence of Phases Content on Pt/TiO2, Pd/TiO2 Catalysts for Degradation of 4-Chlorophenol at Room Temperature
Figure 6
SEM and HRSEM micrographs of (a) undoped TiO2, (b) 3% Pd/TiO2, (c) 3% Pt/TiO2, (d) 1% Pd/TiO2, (e) 3% Pd/TiO2, (f) 5% Pd/TiO2, (g) 1% Pt/TiO2, (h) 3% Pt/TiO2, and (i) 5% Pt/TiO2 samples.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |
(g) |
(h) |
(i) |