Synthesis and Characterization of Nontoxic Hollow Iron Oxide (-) Nanoparticles Using a Simple Hydrothermal Strategy
Figure 2
SEM images showing the hollow spheres of α-Fe2O3 at 12 h reaction time after calcination process: (a) dispersion in ethanol, (b) dispersion in water, (c) high magnification image of sphere showing α-Fe2O3 shell showing the inherent porosity, and (d) EDX mapping showing the Fe content.