Synthesis and Characterization of Nontoxic Hollow Iron Oxide (-) Nanoparticles Using a Simple Hydrothermal Strategy

Figure 6

SEM images showing the growth of hollow spheres of α-Fe2O3 at 24 h reaction time and after calcination: (a) dispersion in ethanol showing the growth mechanism of hollow NPs and (b) hollow NPs showing the pores or broken shell confirming the hollow structure inside the α-Fe2O3 porous shells.
(a)
(b)

We are committed to sharing findings related to COVID-19 as quickly and safely as possible. Any author submitting a COVID-19 paper should notify us at help@hindawi.com to ensure their research is fast-tracked and made available on a preprint server as soon as possible. We will be providing unlimited waivers of publication charges for accepted articles related to COVID-19. Sign up here as a reviewer to help fast-track new submissions.