Summary of dynamic rheological curing.
| Sample | Viscosity at 30°C, μPa·s | Lowest viscosity, μPa·s | Temperature at lowest viscosity, °C | Gel temperature, °C |
| 0 wt.% MMT | 440.3 ± 6.1 | 72.9 ± 15.0 | 68.7 ± 1.4 | 111.8 ± 4.2 | 1 wt.% MMT | 621.1 ± 18.4 | 115.5 ± 34.0 | 75.8 ± 2.9 | 112.0 ± 3.4 | 2 wt.% MMT | 685.1 ± 19.6 | 137.7 ± 19.8 | 69.3 ± 1.3 | 124.1 ± 1.3 | 3 wt.% MMT | 864.7 ± 26.9 | 283.4 ± 14.4 | 59.2 ± 1.7 | 105.7 ± 2.2 |
|
|