Research Article

A Sensor for the Determination of Lindane Using PANI/Zn, Fe(III) Oxides and Nylon 6,6/MWCNT/Zn, Fe(III) Oxides Nanofibers Modified Glassy Carbon Electrode

Figure 6

Effect of scan rate (25–300 mVs−1) on the cyclic voltammograms of (a) GCE/Nylon 6,6/MWCNT/ZnO and (b) GCE/Nylon 6,6/MWCNT/Fe3O4 in 500 μM lindane in 60 : 40 methanol/water containing 0.05 M TBAB. (c) and (d) are the plots of current () against square root of scan rate (mVs−1) for GCE/Nylon 6,6/MWCNT/ZnO and (c) GCE/Nylon 6,6/MWCNT/Fe3O4, respectively.
(a)
(b)
(c)
(d)