Research Article
Sprayed Pyrolyzed ZnO Films with Nanoflake and Nanorod Morphologies and Their Photocatalytic Activity
Table 1
Deposition conditions of the ZnO films.
| Set 1 | Sample name | Concentration (M) | Precursor | Solvent |
| A1A | 0.05 | Zinc acetate | H2O | A2A | 0.1 | A3A | 0.2 |
| C1A | 0.05 | Zinc chloride | H2O | C2A | 0.1 | C3A | 0.2 |
| Set 2 | Precursor zinc acetate 0.05 M | Precursor zinc chloride 0.05 M | Sample name | Solvent: H2O/MeOH | Sample name | Solvent: H2O/MeOH |
| A1A | 100/0 | C1A | 100/0 | A1M25 | 75/25 | C1M25 | 75/25 | A1M50 | 50/50 | C1M50 | 50/50 | A1M75 | 25/75 | C1M75 | 25/75 | A1M100 | 0/100 | C1M100 | 0/100 |
| Set 3 | Sample name | Solvent: H2O/MeOH | Precursor | Concentration |
| AC1A | 100/0 | Zinc acetate + zinc chloride | 0.05 M | AC1M25 | 75/25 | 0.05 M | AC1M50 | 50/50 | 0.05 M | AC1M75 | 25/75 | 0.05 M | AC1M100 | 0/100 | 0.05 M |
|
|