Research Article
Ethylene-Octene Copolymers/Organoclay Nanocomposites: Preparation and Properties
Figure 12
FTIR graph of EOC-17 (Engage 8540) pure and EOC-17 with 5 wt.% Cloisite 93 and details of area 1810 to 1681 cm−1. Picture of change of EOC-17 pure after 46 days of UV degradation. EOC-17 + 5% Cloisite 93 after 46 days of UV degradation.