Research Article
Microstructure and Mechanical Properties of Mg/2 wt.%SiCp Nanocomposite Fabricated by ARB Process
Table 1
Average grain size (
m) at three thickness locations in the Mg/2 wt.%SiC
and monolithic Mg sheets for various ARB cycles.
| ARB cycles | Mg/2 wt.%SiC | Monolithic Mg | 2 | 3 | 4 | 6 | 8 | 11 | 14 | 2 | 3 | 4 | 6 | 8 | 11 | 14 |
| Subsurface | 5.3 | 6.9 | 4.0 | 6.9 | 3.1 | 3.2 | 3.0 | 4.5 | 1.5 | 5.6 | 4.7 | 3.2 | 3.0 | 6.4 | 1/4 thickness | 7.2 | 13.1 | 7.4 | 8.3 | 4.6 | 6.9 | 3.6 | 5.6 | 3.8 | 7.2 | 6.0 | 4.9 | 3.9 | 4.7 | Center | 7.0 | 15.2 | 6.9 | 15.5 | 4.2 | 7.2 | 2.9 | 4.9 | 1.7 | 16.7 | 5.5 | 4.3 | 2.7 | 6.9 | Total | 6.5 | 11.7 | 6.1 | 10.2 | 3.9 | 5.8 | 3.2 | 5.0 | 2.3 | 10.0 | 5.4 | 4.1 | 3.2 | 6.0 |
|
|