Research Article
Microstructure and Mechanical Properties of Mg/2 wt.%SiCp Nanocomposite Fabricated by ARB Process
Table 2
Tensile properties (UTS, 0.2YS%, and
) and microhardness of the Mg/2 wt.%SiC
and monolithic Mg for various ARB cycles.
| ARB cycles | UTS (MPa) | YS (MPa) | (GPa) | Microhardness (HV) | MMNC | Mg | MMNC | Mg | MMNC | Mg | MMNC | Mg |
| 2 | 143.0 | 176.0 | 109.5 | 145.0 | 25.5 | 43.7 | | | 3 | 152.1 | 217.1 | 120.2 | 142.4 | 33.2 | 27.2 | | | 4 | 157.0 | 179.2 | 118.5 | 119.9 | 37.8 | 32.1 | | | 6 | 105.0 | 170.1 | 93.5 | 146.7 | 37.2 | 33.0 | | | 8 | 243.6 | 199.1 | 183.8 | 128.9 | 31 | 30.9 | | | 11 | 262.7 | 60.4 | 189.9 | 49.0 | 45.9 | 37.8 | | | 14 | 291.2 | 237.5 | 250.1 | 130.1 | 64.9 | 21.4 | | |
|
|