Preparation of Spherical Zn-Substituted Tricalcium Phosphate Powder by Ultrasonic Spray-Pyrolysis Technique and Its Characterization
Figure 5
The typical XRD patterns of the fabricated (a) Zn-TCP(0) and (b) Zn-TCP(10) ceramics sintered at (A) 1000°C, (B) 1100°C, (C) 1200°C, and (D) 1300°C.