Preparation of Spherical Zn-Substituted Tricalcium Phosphate Powder by Ultrasonic Spray-Pyrolysis Technique and Its Characterization

Table 1

Nominal composition of the Zn-TCP starting solutions.

Sample/mol·dm−3/mol·dm−3/mol·dm−3 ·/mol·dm−3

Zn-TCP()0.600.400.401.50
Zn-TCP()0.600.400.400.015
Zn-TCP()0.600.400.400.0210
Zn-TCP()0.600.400.400.0315