The Optimum Fabrication Condition of p-Type Antimony Tin Oxide Thin Films Prepared by DC Magnetron Sputtering
Figure 11
The UV-visible spectra of 5%, 10%, and 15% ATO films annealed at 500°C for 2 h after being deposited at room temperature.