Research Article

Electrically Conductive Membranes Obtained by Simultaneous Electrospinning and Electrospraying Processes

Table 5

Volume resistivity measurements before and after immersion and sonication in SDS/water solution.

Volume resistivity (Ω·cm)
MinMaxStd. dev.

Before7.88E + 05
After8.19E + 05