Mean roughness () of study groups after different self-etching techniques.

Subgroups
(self-etching techniques)
HealthyMildModerateSevere

(1) Self-etch (SE)390.83 ± 101.04312.18 ± 100.69296.14 ± 103.87311.30 ± 105.23
(2) NaOCl/SE376.64 ± 100.82335.55 ± 100.11320.57 ± 106.71372.28 ± 105.54
(3) NaOCl/SE + NaAg361.94 ± 100.53369.63 ± 101.95357.48 ± 104.24286.57 ± 103.13

Results show means ± SD expressed in nanometers.