Research Article
Comparative Study of One-Step Cross-Linked Electrospun Chitosan-Based Membranes
Table 1
Summary of cross-linked fiber diameter data obtained from SEM micrographs.
| Membrane | Cross-linker reagent | Cross-linker content (% v/v) | mol GNP : mol NH2 | Fiber diameter (nm) |
| S0.1GTA | GTA | 0.1 | 1 : 136 | 144 ± 40 | S0.3GTA | GTA | 0.3 | 1 : 45 | 159 ± 91 | S0.5GTA | GTA | 0.5 | 1 : 27 | 147 ± 35 | S0.1TPP | TPP | 0.1 | 1 : 83 | 132 ± 68 | S0.3TPP | TPP | 0.3 | 1 : 28 | 119 ± 49 | S0.5TPP | TPP | 0.5 | 1 : 17 | 133 ± 61 | S | — | 0.0 | — | 131 ± 41 | S0.1GNP | GNP | 0.1 | 1 : 51 | 119 ± 33 | S0.2GNP | GNP | 0.2 | 1 : 25 | 91 ± 24 | S0.3GNP | GNP | 0.3 | 1 : 17 | 86 ± 25 | S0.4GNP | GNP | 0.4 | 1 : 13 | 80 ± 29 | S0.5GNP | GNP | 0.5 | 1 : 10 | 58 ± 17 | SUV | UVA | 0 | — | 98 ± 20 | S0.1GNPUV | GNP+UVA | 0.1 | 1 : 51 | 95 ± 28 | S0.2GNPUV | GNP+UVA | 0.2 | 1 : 25 | 91± 33 | S0.3GNPUV | GNP+UVA | 0.3 | 1 : 17 | 56 ± 12 | S0.4GNPUV | GNP+UVA | 0.4 | 1 : 13 | 108 ± 26 | S0.5GNPUV | GNP+UVA | 0.5 | 1 : 10 | 107 ± 30 |
|
|