Thermal Stability of Cryomilled Al-Mg-Er Powders

Table 1

Composition of atomized and 30-hour milled powders (wt.%).

ElementMgErTiFeNiTlSiSbZnCr

Atomized 0.1 Er5.290.120.190.070.010.150.070.050.040.00
Atomized 0.5 Er5.400.550.060.040.000.040.070.010.020.00

Milled 0.1 Er4.650.080.260.390.170.060.050.030.020.04
Milled 0.5 Er4.480.440.010.160.030.000.050.010.020.03