Research Article
Preparation of Cerium Dioxide Layers on Titanium by Electrodeposition with Organic Solution
Figure 2
XPS spectra of (a) cerium nitrate precursor dried on Ti and layers on Ti electrodeposited at 31.6 V (b) as prepared and (c) calcined at 700 K for 30 min.