Research Article

Preparation of Cerium Dioxide Layers on Titanium by Electrodeposition with Organic Solution

Table 1

Elemental composition (atomic %) obtained from XPS spectra for cerium nitrate precursor and electrodeposition layers.

Major (atomic %)Cerium nitrate precursorLayers
As-preparedCalcined at 700 K for 30 min

Ce4.613.016.9
O61.952.658.8
C20.332.324.3
N13.22.1

Titanium excluded in elemental compositions.