Research Article
Effect of Drying Temperature on Iron Fischer-Tropsch Catalysts Prepared by Solvent Deficient Precipitation
Table 3
Catalyst surface area, pore volume, and average pore diameter.
| Catalyst | BET surface area (m2/g) | Pore volume (cm3/g) | Average pore diameter (nm) |
| C80 | 71 | 0.155 | 9.8 | C100 | 56 | 0.107 | 8.4 | C115 | 23 | 0.048 | 9.8 | C130 | 54 | 0.203 | 19.4 | C130b | 87 | 0.163 | 7.9 | C150 | 34 | 0.069 | 8.6 | C150NP | 24 | 0.059 | 13.0 |
|
|