Optimal Zn-Modified Ca–Si-Based Ceramic Nanocoating with Zn Ion Release for Osteoblast Promotion and Osteoclast Inhibition in Bone Tissue Engineering

Figure 1

Morphology of Ti, Zn/Ca (0), Zn/Ca (0.1), Zn/Ca (0.3), and Zn/Ca (0.5), respectively. The bar is 1 mm in 10x magnification and the bar is 2 μm in 5000x magnification, respectively.