Research Article
Elastomeric Nanocomposite Based on Exfoliated Graphene Oxide and Its Characteristics without Vulcanization
Table 3
Effect of water volume in the GO suspension on the coagulation time of the GO/NBR nanocomposite.
| Distilled water volume (mL) | Coagulation time (min) | GO dispersion | Coagulation state of GO/NBR |
| 10 | 0.5 | Incomplete | Coagulated | 8 | 1 | Incomplete | Coagulated, melted | 6 | 15 | Partially | Viscos, coagulated | 4 | 35 | Complete | Viscos solution | 2 | 55 | Max. disp | Low viscous solution |
|
|