The electrical conductivity of unvulcanized GO/NBR nanocomposites at different GO loadings.

GO loading
wt% (g)
Current
(A)
Resistivity (Ωcm)Conductivity
(S/cm)

0.00.9839.1525.54
0.20.7650.5119.80
0.41.4626.2938.03
0.81.8820.4348.94
1.01.9319.9150.22