Research Article
Formation and Investigation of Electrospun PLA Materials with Propolis Extracts and Silver Nanoparticles for Biomedical Applications
Table 2
Viscosity of PLA solutions and diameter of electrospun PLA microfibers.
| Sample code | Composition of electrospun solutions | Viscosity , s | Average diameter of electrospun PLA microfibers, nm ± |
| A | Pure PLA solution (concentration of PLA in solution wt%) | 7,3 ± 0.03 | 168 ± 29 | B | PLA with 10 wt% ethanol (PLA wt%) | 6,5 ± 0.5 | 318 ± 40 | C | PLA with 20 wt% ethanol (PLA wt%) | 6,3 ± 0.3 | 370 ± 30 | D | PLA with 10 wt% PEE (PLA wt%) | 7,0 ± 0.3 | 282 ± 25 | E | PLA with 20 wt% PEE (PLA wt%) | 6,8 ± 0.3 | 371 ± 25 | F | PLA with 5 wt% colloidal solution of AgNPs (PLA wt%) | 7,1 ± 0.4 | 254 ± 25 | G | PLA with 10 wt% PEE and 5 wt% colloidal solution of AgNPs (PLA wt%) | 7,0 ± 0.1 | 280 ± 29 | H | PLA with 20 wt% PEE and 5 wt% colloidal solution of AgNPs (PLA wt%). | 7,1 ± 0.3 | — |
|
|
The absolute error.
|