Research Article
Room Temperature Ferromagnetic and Optical Properties of Chrome Doped ZnS Nanorods Prepared by Hydrothermal Method
Table 1
Parameters of the XRD patterns for Zn
Cr
S (
, 0.01, 0.03, and 0.05) nanorods.
| Sample | 2θ (°) | FWHM (°) | (Å) | (Å) | (Å) | Cell volume (Å3) | (nm) |
| Pure ZnS | 28.500 | 0.269 | 3.129 | 3.829 | 6.258 | 79.45 | 30 | Zn0.99Cr0.01S | 28.520 | 0.213 | 3.127 | 3.828 | 6.254 | 79.36 | 34 | Zn0.97Cr0.03S | 28.618 | 0.245 | 3.117 | 3.799 | 6.233 | 77.90 | 36 | Zn0.95Cr0.05S | 28.539 | 0.258 | 3.125 | 3.824 | 6.250 | 79.15 | 39 |
|
|