Research Article
Room Temperature Ferromagnetic and Optical Properties of Chrome Doped ZnS Nanorods Prepared by Hydrothermal Method
Table 2
Band gap and magnetic moments of Zn
Cr
S (
, 0.01, 0.03, and 0.05) nanorods.
| Sample | Band gap (eV) | Magnetic moments (emu/g) | Saturation magnetization | Remanent magnetization (10ā4) | Coercivity (Oe) |
| Pure ZnS | 3.729 | 0.0117 | 6.415 | 46.71 | Zn0.99Cr0.01S | 3.737 | 0.0111 | 5.122 | 40.26 | Zn0.97Cr0.03S | 3.743 | 0.0097 | 5.339 | 41.22 | Zn0.95Cr0.05S | 3.732 | 0.0105 | 5.376 | 42.74 |
|
|