Silver lixiviation test during the photocatalytic degradation of ATL at 10 ppm and pH normal.

SampleAg concentration (ppm)Lixiviation (%)

Ag@H2Ti3O7 0.50.00530.4
Ag@H2Ti3O7 1.00.02821.2
Ag@H2Ti3O7 2.50.08056.4