Research Article
Role of Laser Power, Wavelength, and Pulse Duration in Laser Assisted Tin-Induced Crystallization of Amorphous Silicon
Figure 4
Typical optical images of the samples’ surface after laser irradiation with optical power = 0–5 × 104 W/cm−2 (a) and = 8.2 × 104 W/cm−2 (b). Irradiation wavelength was = 1.07 μm and pulse duration = 150 ns.
(a) |