Research Article
Role of Laser Power, Wavelength, and Pulse Duration in Laser Assisted Tin-Induced Crystallization of Amorphous Silicon
Figure 8
Optical images of a sample surface without laser irradiation (a) and irradiated with laser at 535 nm, 10 ns pulse duration, and optical power of I = 2–20 × 106 W/cm−2 (b).
(a) |